The transportation demands in our growing hydrogen (H2) economy requires robust storage systems. The current commercially implemented technology in fuel cell cars relies on the well-established technology of hydrogen gas compressed to 350–700 bar, depending on the application. The compressed gas tanks in use today are bulky and cost intensive. To address this challenge, material-based storage is one of the long-term alternatives considered and constitutes the focus of this talk.Material-based storage is broadly defined as hydrogen bound to solid materials, with its binding strength varying from physisorption to porous materials, such as zeolites and metal organic frameworks, to chemisorption in (complex) metal hydrides. The ultimate targets set by the U.S. Department of Energy for this technology include a system gravimetric capacity of 6.5 wt% and volumetric capacity of 40 g/L at 100 bar, operating temperatures ranging between -40 C and +40 C and adsorption/desorption timescales of < 5 min. Storage in the form of physisorbed or chemisorbed hydrogen has guided the materials research, which metal-organic framework and (complex) metal hydrides being the most promising materials classes. A variety of these materials have met one or more of the targets, but it has remained elusive for a single material system to meet all these stringent requirements. Nano-encapsulation and low-concentration chemical additives have previously been employed separately to overcome such challenges. Functionalization via atomic layer deposition (ALD), however, offers unique characteristics that make it suitable for both, nano-encapsulation and “doping” with low-concentration additives. This deposition technique has sub-monolayer thickness control, is highly conformal in high-surface area materials and is self-limiting, i.e., once the gas-phase precursor reacts with the available surface sites, the surface reactions stop.In this presentation, we will showcase examples where ALD, more generally vapor-phase functionalization, on (complex) metal hydrides and organic frameworks has improved the material properties for H2 storage. In our first study, Al2O3 was deposited on magnesium borohydride, Mg(BH4)2, at room temperature using trimethylaluminum (TMA) and water. From our findings, encouraging initial results were obtained: the H2 desorption temperature was lowered by 60–120 ˚C, the desorbed gravimetric H2 capacity at temperatures < 250 ˚C was doubled, and the desorption kinetics increased by a factor of ~6 compared to uncoated Mg(BH4)2. However, hydrolysis reactions caused by residual surface -OH groups from the ALD water-pulse degraded the sample substantially. Through this study, the use of TMA was observed to be highly reactive with the Mg(BH4)2 surface species, leading to the strategy of exposing the sample only to TMA. The relative mole fraction of the vapor-phase additive can be precisely controlled with the number of TMA pulses and pulse duration. By tuning these parameters, we show in our second study that 10 pulses of TMA at ambient conditions were able to decrease the H2 desorption temperature by ~100 ˚C while retaining <95 % of its H2 capacity. We applied this approach with other additives such as BBr3, TiCl4 and tetrahydrofuran, and demonstrate that this unique approach opens the door to a new class of molecular additives and catalysts which cannot easily be introduced with conventional mechano-chemical or solvent-based techniques for (complex) metal-hydrides. In the case of metal organic frameworks, ALD is a promising technique to functionalize the pores with metal atoms or functional groups able to tune the gas selectivity and binding energy, for which ~15 kJ/mol has been established as the optimal value for H2 storage in sorbent materials.Vapor-phase techniques such as ALD have numerous benefits over other functionalization tools for H2 storage materials opening innumerable opportunities to the field. To exploit these opportunities, the current limitations on room temperature and water-less ALD processes needs to be overcome which will greatly expand the possibilities of encapsulation and incorporation of additives for organic frameworks and (complex) metal hydrides.

Similar Papers
  • Research Article
  • Citations128

Targeted Single-Site MOF Node Modification: Trivalent Metal Loading via Atomic Layer Deposition

  • Jul 02, 2015
  • Chemistry of Materials
  • In Soo Kim +10
  • Research Article
  • Citations84

Regioselective Atomic Layer Deposition in Metal-Organic Frameworks Directed by Dispersion Interactions.

  • Oct 10, 2016
  • Journal of the American Chemical Society
  • Leighanne C Gallington +11
  • Research Article
  • Citations132

An overview of reactive hydride composite (RHC) for solid-state hydrogen storage materials

  • Aug 01, 2021
  • International Journal of Hydrogen Energy
  • N.A Ali +2
  • Research Article
  • Citations237

Brønsted-Lowry Acid Strength of Metal Hydride and Dihydrogen Complexes.

  • Mar 10, 2016
  • Chemical Reviews
  • Robert H Morris
  • Research Article

Can Trimethylaluminum (TMA) Alone Serve as a Vapor Precursor for Surface Functionalization of Battery Materials?

  • Nov 24, 2025
  • Electrochemical Society Meeting Abstracts
  • Donghyeon Kang +6
  • Research Article
  • Citations174

Atomically Precise Growth of Catalytically Active Cobalt Sulfide on Flat Surfaces and within a Metal-Organic Framework via Atomic Layer Deposition.

  • Aug 04, 2015
  • ACS Nano
  • Aaron W Peters +3
  • Research Article

Application of Atomic Layer Deposition for Fabrication of Solar Cells

  • Sep 01, 2019
  • Electrochemical Society Meeting Abstracts
  • Karol Frohlich +11
  • Research Article
  • Citations28

Air, Water Vapor, and Aerosol Transport through Textiles with Surface Functional Coatings of Metal Oxides and Metal-Organic Frameworks.

  • Jun 05, 2019
  • ACS Applied Materials &amp; Interfaces
  • Natalie L Pomerantz +8
  • Research Article

Elucidating the Surface Chemistry of Atomic Layer Deposition on Complex Metal Oxide Cathode Materials

  • Oct 19, 2021
  • Electrochemical Society Meeting Abstracts
  • Pragathi Darapaneni +2
  • Research Article

Interfacial oxide and other species in trimethylaluminum-pretreated atomic layer deposition-Al2O3/GaN characterized by sputter-assisted ToF-SIMS

  • Jun 25, 2025
  • Journal of Vacuum Science &amp; Technology A
  • B D Rummel +7
  • Research Article
  • Citations223

Ultra-Fast Degradation of Chemical Warfare Agents Using MOF-Nanofiber Kebabs.

  • Oct 06, 2016
  • Angewandte Chemie International Edition
  • Junjie Zhao +9
  • Research Article
  • Citations49

Probing the Atomic-Scale Structure of Amorphous Aluminum Oxide Grown by Atomic Layer Deposition.

  • Apr 20, 2020
  • ACS Applied Materials &amp; Interfaces
  • Matthias J Young +9
  • Research Article
  • Citations5

ChemInform Abstract: Crystallinity of Inorganic Films Grown by Atomic Layer Deposition: Overview and General Trends

  • Feb 26, 2013
  • ChemInform
  • Ville Miikkulainen +3
  • Supplementary Content

Addressing Thermodynamic Inefficiencies of Hydrogen Storage in Transition Metal Hydrides

  • Jan 01, 2019
  • Nicholas J Weadock
  • Research Article
  • Citations28

Effect of Complex Metal Hydrides on the Elimination of Hydrochloric Acid Exhaust Products from High‐Performance Composite Solid Propellants: A Theoretical Analysis

  • May 28, 2020
  • Propellants, Explosives, Pyrotechnics
  • Fateh Chalghoum +3
Cactus Communications logo

Copyright 2026 Cactus Communications. All rights reserved.