- Research Article
9
- 10.1143/jjap.51.041104
Oxidation of Silicon Utilizing a Microwave Plasma System: Electric-Stress Hardening of SiO2 Films by Controlling the Surface and Interface Roughness
- Mar 23, 2012
- Japanese Journal of Applied Physics
- Yoshiro Kabe + 2 more +2
Electric-stress hardening of silicon dioxide (SiO2) films under high electric field stresses was studied. SiO2 films were formed by two-step oxidation utilizing thermal oxidation and plasma oxidation. This process has the advantages of both oxidation processes: the low degradation rate of thermal oxidation and the flat SiO2 surface and SiO2/Si interface obtained by plasma oxidation. Time-dependent dielectric breakdown and stress-induced leakage current were measured to evaluate the degradation rate and the breakdown lifetime of the oxides. Atomic force microscopy was used to evaluate the roughnesses of the SiO2 surface and interface. The two-dimensional degradation distribution under a current stress was investigated by the stress-induced etched-oxide surface roughness method. Atomically uniform SiO2 was found to suppress the generation of local weak spots under current stress. We conclude that using an appropriate combination of the oxidation processes can reduce the degradation and enhance the breakdown lifetimes of SiO2 films.
Read more