- Book Chapter
- 10.1016/b978-0-323-85742-0.00003-2
Chapter 3 - Biofouling
- Jan 01, 2024
- Corrosion and Corrosion Protection of Wind Power Structures in Marine Environments
- Andreas Momber
Publications from 2021 to 2026
Showing 10 of 12 papers
Chapter 3 - Biofouling
Chapter 9 - Inspection, maintenance, and repair
Effects of compressive damage on the corrosion protection performance of offshore wind power coating systems
Abstract Damage to multilayer organic coating systems due to compressive loads can deteriorate the corrosion protection performance of the coatings under offshore exposure. The contribution is concerned with statistical investigations into the effects of load‐based and coating‐based factors on the protection performance of different coating systems. Accelerated cyclic laboratory tests (ISO 12944‐9) were performed on four multilayer coating systems, and the results were statistically analyzed. Results of analysis of variance investigations revealed that the effects on the anticorrosive performance of the coatings (anticorrosive effect [AE]) were dominated by coating‐based factors, namely coating system and total dry film thickness. These factors could explain 86% of all effects. Coating system was the only extremely significant factor. Load‐based factors did not deliver notable effects (5%). Except for the contact stiffness, these factors were insignificant. The load intensity was insignificant for all target parameters (blistering, delamination, AE). Coating regions, plastically deformed during the compression tests, did not lead to a reduction in the protection performance.
Read moreMeasurement methods and fractal dimensions of blast-cleaned steel substrates
ABSTRACT Morphological parameters of steel substrates determine the adhesion of coatings and adhesives. Three different assessment methods (cross section image, contact stylus instrument, and stripe light projection) were applied to blast-cleaned substrates. A total of 12 surface configurations were generated with different abrasive materials. The fractal dimensions were estimated by means of the box-counting method. Design of experiment and ANOVA were applied to statistically analyze the relationships. Factors included abrasive type, surface preparation grade, surface roughness, and surface profile measurement method. Similar relative trends for the fractal dimensions resulted for the three measurement methods. The normalized values of the fractal dimensions were approximately twice as high for the cross section profiles compared to the ones from contact stylus and stripe light projection. Fractal values derived from contact stylus measurements showed the highest repeatability, whereas those derived from cross section images showed the lowest repeatability.
Read moreThe corrosion of carbon steel under delaminating repair coatings after long‐term marine splash zone exposure
Abstract Organic repair coatings are applied to repair areas of previously coated low‐carbon steel samples, and the samples are exposed to the splash zone in an offshore environment (Helgoland, North Sea) for 57 months. The volume loss of the steel underneath the delaminated coating is estimated with a three‐dimensional optical stripe line projection. The samples show a small variation in the degree of delamination (22%) only. The steel volume loss values, in contrast, range between 164 × 109 and 320 × 109 µm³, which is a variation of 196%. The degree of delamination of the scribed coatings does not mirror the corrosion of the steel underneath the delaminated sections. The coating with the widest degree of delamination exhibits the lowest steel volume loss due to corrosion. A good scribe performance of a coating is, therefore, no guarantee for a low corrosion loss nor for a low local corrosion depth in the steels to be protected.
Read moreThe assessment of fractal dimensions with the direct use of scanning electron microscopy (SEM) images from blast-cleaned steel substrates
Morphological parameters of substrate surfaces determine the adhesion of coatings and pressure-sensitive adhesives. This paper is concerned with the assessment of fractal parameters by means of the direct use of scanning microscope images (SEM) of blast-cleaned substrates. Mild steel samples were prepared with different abrasive materials. Images were taken from a total of 12 surface configurations with a scanning electron microscope. The fractal dimensions of the surfaces were estimated on four different image sizes with and without the use of a median filter by means of the box-counting method. All tests were performed twice to evaluate accuracy and repeatability of the assessment procedure. Design of Experiment (DoE) was applied in order to statistically analyze the relationships. The factors considered included abrasive type, surface preparation grade and surface roughness. Independently on filter and image size, no meaningful regression model could be established. Neither main effects nor interactive effects of the factors on the fractal dimensions could be identified. The deviations in the fractal dimension were larger for two measurements on a given factor combination than the deviations for two measurements at different factor combinations. The direct use of SEM images is, therefore, not practical for the estimation of fractal dimensions of blast-cleaned steel substrates.
Read moreThe corrosion protection performance of repair coatings for offshore wind power constructions after long‐term splash zone site exposure
Abstract Four organic repair coatings are applied to low‐carbon steel samples prepared with rotating wire blasting, and the samples are exposed to the splash zone in an offshore environment (Helgoland, North Sea) for 57 months. The relationships between aging procedure, coating type, and corrosion protection performance are systematically investigated with statistical methods. Design of experiments and analysis of variance are used to rank the parameter effects. Response parameters are the degree of coating delamination and pull‐off strength. Extremely significant interactions are found between aging procedure and delamination and between coating type and pull‐off strength. An extremely significant interaction between the factors aging procedure and coating type is found for the pull‐off strength only. The degree of delamination is alternatively discussed in terms of the delaminated area. Acceleration factors, calculated from results of the site exposure tests and of accelerated cyclic laboratory test, range between 5.2 and 8.6.
Read moreEffects of adhesive type on the mechanical properties of adhesive joints between polyurethane top coats and polyurethane-based adhesives after accelerated atmospheric ageing
Nachträgliches klebtechnisches Fügen von Haltern auf Beschichtungen mit ungenügender Haftfestigkeit
Abstract Es wird ein Verfahren zum nachträglichen klebtechnischen Fügen von Haltern beschrieben, das auch für Bereiche mit ungenügender Haftung der Beschichtung zum Substrat eine hohe mechanische Beständigkeit unter Zugscherbeanspruchung gewährleistet. Das Verfahren ermöglicht eine umweltverträgliche, nahezu emissionsfreie und materialschonende örtliche Vorbereitung von Beschichtungsbereichen mit ungenügender Haftung zur Stahloberfläche. Eine integrierte mechanisierte Haftfestigkeitsmessung gestattet eine objektive Bewertung der Tragfähigkeit von beschichteten Oberflächen und eine Entscheidung darüber, ob das klebtechnische Fügen auf der beschichteten oder der teilweise freigelegten Stahloberfläche erfolgen kann.
Read morePerformance and integrity of protective coating systems for offshore wind power structures after three years under offshore site conditions